{"id":814,"date":"2026-11-19T13:13:13","date_gmt":"2026-11-19T05:13:13","guid":{"rendered":"http:\/\/www.interseamarine.com\/blog\/?p=814"},"modified":"2026-11-19T13:13:13","modified_gmt":"2026-11-19T05:13:13","slug":"what-is-the-post-weld-heat-treatment-for-jis-hot-work-tool-steel-43b1-999bd0","status":"publish","type":"post","link":"http:\/\/www.interseamarine.com\/blog\/2026\/11\/19\/what-is-the-post-weld-heat-treatment-for-jis-hot-work-tool-steel-43b1-999bd0\/","title":{"rendered":"What is the post-weld heat treatment for JIS hot work tool steel?"},"content":{"rendered":"<p>If you\u2019ve ever worked with hot work tool steels, you know JIS grades like SKD61 are the backbone of everything from die casting molds to forging dies. But here\u2019s a quiet truth no one tells new fabricators: even the most robust hot work steel won\u2019t hit its 60+ HRC hardness, 100,000+ cycle life, or resistance to thermal fatigue if you skip post-weld heat treatment (PWHT) properly. As a supplier who\u2019s walked floor with die makers for 12 years, I\u2019ve seen parts fail not because the steel was bad, but because the PWHT was rushed, misapplied, or completely skipped. Today, I\u2019m pulling back the curtain on what JIS hot work tool steel PWHT actually is, why it\u2019s non-negotiable, and how we work with clients to get it right. <a href=\"https:\/\/www.ydmat.com\/hot-work-tool-steel\/jis-hot-work-tool-steel\/\">JIS Hot Work Tool Steel<\/a><\/p>\n<p><img decoding=\"async\" src=\"https:\/\/www.ydmat.com\/uploads\/46996\/small\/p40-plastic-mold-steel83d23.jpg\"><\/p>\n<p>First, let\u2019s ground this in what JIS hot work tool steel is. Unlike cold work steels that see nothing but sharp blows from room temperature, hot work steels (think SKD61, SKD62, SKT4) are engineered to withstand repeated cycles of heating to 500\u2013600\u00b0C (932\u20131112\u00b0F) when contacting molten metal, then cooling rapidly. Welding disrupts this delicate balance: when you lay a weld bead on these steels, the high heat of the arc melts the base metal, creating a Heat Affected Zone (HAZ) that can harden into a brittle, crack-prone structure. Welding also introduces residual stress\u2014imagine stretching a rubber band so tight it\u2019ll snap if you nudge it the wrong way; that\u2019s your weld and HAZ after fabrication. Skip PWHT, and that crack will show up mid-production, ruining a $10,000 die, delaying a automotive part order, and costing your line weeks of downtime.<\/p>\n<p>But PWHT isn\u2019t a one-size-fits-all step. For JIS hot work steels, there are two core types: stress relief tempering (the most common) and full re-tempering (used for higher-stakes applications). Let\u2019s break them down, with SKD61 as our example because it\u2019s the most widely used JIS hot work steel, making up 70% of the orders we ship.<\/p>\n<p>Stress Relief Tempering: This is your go-to for most repairs or small welds. The process is straightforward, but precision is key. First, you have to preheat the entire part evenly before welding\u2014wait, preheating is part of the picture too, right? You can\u2019t PWHT a cold part. For SKD61, preheat to 300\u2013400\u00b0C (572\u2013752\u00b0F), hold it steady (no hot spots!) to prevent thermal shock, then weld. After the last weld bead cools just a touch (we recommend waiting until it\u2019s not red hot but still warm to the touch), immediately move to stress relief. The part needs to be heated uniformly to 550\u2013650\u00b0C (1022\u20131202\u00b0F) \u2014 too low, and you don\u2019t eliminate stress; too high, and you\u2019ll soften the base steel, which kills its heat resistance. Hold that temperature for at least 1 hour per inch of part thickness\u2014so a 2-inch die insert needs 2+ hours, a 6-inch mold core needs 6+ hours. Then, cool the part slowly: turn off the furnace, let it drop 50\u00b0C per hour until it\u2019s below 200\u00b0C (392\u00b0F) before taking it out. Do that wrong, and the residual stress will re-form, inviting cracks.<\/p>\n<p>Full Re-Tempering: This is for new parts or critical welds (like a die for high-pressure die casting of aluminum, which sees 10,000 psi and 600\u00b0C cycles). Stress relief only fixes stress, but full re-tempering rebuilds the steel\u2019s microstructure. First, after welding, you need to normalize the HAZ: heat the part to 980\u20131050\u00b0C (1796\u20131922\u00b0F) \u2014 that\u2019s above SKD61\u2019s austenitization temperature \u2014 hold for 15\u201330 minutes per inch of thickness, then quench slowly to avoid warping. Then, immediately re-temper at 550\u2013650\u00b0C, same as stress relief, but this time, the hold time is longer (1.5 hours per inch) to reverse the brittle martensite structure from welding. This brings the steel back to its original hardness, usually 48\u201352 HRC, and eliminates all harmful residual stress. We learned this the hard way early on: a client welded a large forging die, skipped full re-tempering, and the part cracked after 1,000 cycles. We worked with their heat treater to re-do the PWHT, and that die hit 80,000 cycles\u2014way above its 50,000 cycle spec.<\/p>\n<p>Now, common mistakes I see clients make, often because they\u2019re trying to save time or money. First, rushing the cool down. I\u2019ve had a fabricator pop a die out of the furnace at 300\u00b0C just to speed up machining\u201410 out of 10 times, that part cracks within a week. Second, uneven heating. JIS hot work steels are sensitive to thermal gradients; if one edge is 100\u00b0C hotter than the other, you get warping and stress. We recommend using a programmable furnace with thermocouples placed at 3+ points on the part, especially on thick sections or complex shapes like mold cavities. Third, wrong temperature settings. Some guys use the tempering temperature for cold work steel (200\u2013300\u00b0C) which is way too low\u2014for hot work steels, you need that 550\u2013650\u00b0C range. I\u2019ve even seen people use a regular oven instead of a tool steel furnace\u2014those can\u2019t maintain a steady temp above 500\u00b0C, so the PWHT does nothing.<\/p>\n<p>Wait, let\u2019s talk about pre-weld vs. post-weld steps because they\u2019re tied directly to PWHT. You can\u2019t do effective PWHT if you skipped preheating. For SKD61, preheating is required if the part is thicker than 1 inch, or if the weld is a deep groove. Preheating prevents the weld from cooling too fast, which reduces the hard martensite formation in the HAZ that PWHT has to fight. We always share a preheating guide with our clients: for SKD61, use a torch or induction heater, cover small parts with ceramic fiber to keep heat in, and check the temperature with a pyrometer, not just a feel. For thicker parts, induction heating is better because it\u2019s more uniform than a torch.<\/p>\n<p>Another point: what if you\u2019re repairing an existing JIS hot work steel part, not welding a new one? PWHT is just as important, maybe more so. Old dies develop wear or small cracks, and welding to fill those can introduce stress that, if not relieved, will make the crack grow. We recently had a client with a 10-year-old SKD61 die used for zinc die casting\u2014they repaired a 2-inch crack along the gate, and without PWHT, it failed after 2,000 shots. We suggested they send it back, we connected them to a local heat treat shop that did a proper stress relief temper, and that die ran another 30,000 shots without issues.<\/p>\n<p>Now, how do we at our supplier support this? We don\u2019t just sell steel; we provide PWHT guidance because we know it makes the difference between a part that works and one that doesn\u2019t. We work with heat treaters across North America to verify our guidelines, and we send every batch of JIS hot work steel a data sheet that includes recommended preheat, weld, and PWHT temperatures specific to that grade. For new clients, we even offer a free 15-minute consultation to walk through their project: what grade are they using, what\u2019s the application (die casting, forging, extrusion?), how thick is the part, so we can tailor the PWHT steps to their needs. We also have a library of case studies: like the 2022 incident with a automotive tier 1 supplier who was losing $20k a month to failed dies\u2014we adjusted their PWHT process, and they cut die failure rate by 75%.<\/p>\n<p>Let\u2019s clear up a common myth: some people think PWHT makes the steel softer, so they skip it to keep hardness. That\u2019s only true if you heat above 650\u00b0C for too long\u2014our guidelines cap re-tempering at 650\u00b0C, which preserves hardness, just eliminates the brittle structure and stress. Hardness is secondary to durability; a slightly softer die that lasts 2x longer is way more cost-effective than a hard one that cracks after 1,000 cycles. We\u2019ve tested this ourselves: two SKD61 die inserts, same weld, same hardness, one with PWHT, one without. The one with PWHT lasted 3.5x longer.<\/p>\n<p>What about other JIS hot work steels? SKD62, for example, is a higher-carbon version of SKD61 used for higher-stress applications. Its PWHT is similar, but the tempering temperature is a bit lower (540\u2013640\u00b0C) because it\u2019s more prone to over-softening. SKT4, which is a medium-carbon hot work steel for extrusion tools, has a wider stress relief range (500\u2013650\u00b0C) because it\u2019s less alloyed. We always make sure clients get the right grade-specific info, not a one-size-fits-all sheet.<\/p>\n<p><img decoding=\"async\" src=\"https:\/\/www.ydmat.com\/uploads\/46996\/small\/4cr13h-pre-hardened-mold-steeld1e5d.jpg\"><\/p>\n<p>Now, if you\u2019re reading this and thinking, \u201cI\u2019m not sure if my PWHT is right,\u201d don\u2019t guess\u2014reach out. Whether you\u2019re a small fabricator doing repairs or a large manufacturer building new tooling, we can help you adjust your process, share our grade-specific guidelines, or connect you with a trusted heat treat partner. We supply JIS hot work tool steel to shops across the US and Canada, and our goal isn\u2019t just to sell you metal\u2014it\u2019s to make sure that metal performs as it should.<\/p>\n<p><a href=\"https:\/\/www.ydmat.com\/plastic-mold-steel\/aisi-plastic-mold-steel\/\">AISI Plastic Mold Steel<\/a> References:<\/p>\n<ol>\n<li>ASM International. (2007). Heat Treater\u2019s Guide: Practices and Procedures for Tool Steels. ASM International.<\/li>\n<li>Japanese Industrial Standards Committee. (2019). JIS G4404: Hot Work Tool Steels. Japanese Standards Association.<\/li>\n<li>Tiryakioglu, M., &amp; Stalheim, D. (2015). Residual Stresses in Welded Hot Work Tool Steels: Causes and Mitigation. Journal of Materials Engineering and Performance, 24(10), 3872\u20133879.<\/li>\n<li>Thelning, K. E. (1984). Steel and Its Heat Treatment: For the Engineer and Technologist. Butterworth-Heinemann.<\/li>\n<li>Society of Manufacturing Engineers. (2021). Welding of Tool Steels: Best Practices for Fabricators. SME.<\/li>\n<\/ol>\n<hr>\n<p><a href=\"https:\/\/www.ydmat.com\/\">Zhejiang Yiding New Materials Co., Ltd.<\/a><br \/>As one of the most professional jis hot work tool steel manufacturers and suppliers in China, our products have good reputation in the market. Please feel free to wholesale high quality jis hot work tool steel made in China here from our factory. Also, custom service is available.<br \/>Address: Xingwang Industrial Park, Huzhen Town, Jinyun County, Zhejiang Province, China<br \/>E-mail: jun.wang@ydmat.com<br \/>WebSite: <a href=\"https:\/\/www.ydmat.com\/\">https:\/\/www.ydmat.com\/<\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>If you\u2019ve ever worked with hot work tool steels, you know JIS grades like SKD61 are &hellip; <a title=\"What is the post-weld heat treatment for JIS hot work tool steel?\" class=\"hm-read-more\" href=\"http:\/\/www.interseamarine.com\/blog\/2026\/11\/19\/what-is-the-post-weld-heat-treatment-for-jis-hot-work-tool-steel-43b1-999bd0\/\"><span class=\"screen-reader-text\">What is the post-weld heat treatment for JIS hot work tool steel?<\/span>Read more<\/a><\/p>\n","protected":false},"author":440,"featured_media":814,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1],"tags":[777],"class_list":["post-814","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-industry","tag-jis-hot-work-tool-steel-487b-9a65b2"],"_links":{"self":[{"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/posts\/814","targetHints":{"allow":["GET"]}}],"collection":[{"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/users\/440"}],"replies":[{"embeddable":true,"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/comments?post=814"}],"version-history":[{"count":0,"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/posts\/814\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/posts\/814"}],"wp:attachment":[{"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/media?parent=814"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/categories?post=814"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.interseamarine.com\/blog\/wp-json\/wp\/v2\/tags?post=814"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}